Flake-Filled Bis-A Lining

System Components
Features
- Abrasion-resistant
- Broad chemical resistance
- Better recoat times
Performance Data
| Test Method | Results |
|---|---|
| Compressive Strength (ASTM C579) | 9,000-9,500 psi (62-66 MPa) |
| Flexural Strength (ASTM C580) | 5,000-5,200 psi (34-36 MPa) |
| Shore D Hardness (ASTM D2240) | 75-80 |
| Taber Abrasion* (ASTM D4060) | 90 mg |
| Tensile Strength (ASTM C307) | 2,500-3,000 psi (17-20.7 MPa) |